深海油气田输送用X65/Inconel 625双金属复合板热变形行为及热轧工艺 |
| 刘庚, 单以银, 严伟, 苏锐, 任毅, 史显波 |
|
Thermal Deformation Behavior and Hot Rolling Process of X65/Inconel 625 Bimetal Composite Plate for Deep Sea Oil and Gas Field Transportation |
| LIU Geng, SHAN Yiyin, YAN Wei, SU Rui, REN Yi, SHI Xianbo |
| 图1 热压缩变形工艺示意图、热压缩方向和试样初始组织 |
| Fig.1 Schematic of the hot compressive deformation processes (a) and compression direction and initial microstructure (b) (unit: mm. T—temperature, t—time) |
|