高氮316LN奥氏体不锈钢的微观组织调控与摩擦学行为
赵利媛, 李小琳, 丁然, 邓想涛, 冯浩, 李花兵, 王海丰

Microstructural Control and Tribological Behavior of High-Nitrogen 316LN Austenitic Stainless Steel
ZHAO Liyuan, LI Xiaolin, DING Ran, DENG Xiangtao, FENG Hao, LI Huabing, WANG Haifeng
图3 不同组织高氮钢的低温摩擦系数曲线
Fig.3 Coefficient of friction (CoF) curves of high-nitrogen steels with different structures at cryogenic temperatures
(a) non-recrystallized (NG) structure
(b) heterogeneous (HS) structure
(c) fully recrystallized (CG) structure