凝固条件对DD6单晶高温合金组织演化的影响
谢洪吉, 李嘉荣, 骆宇时, 郑素杰, 骆凯伦

Effect of Solidification Conditions on Microstructure Evolution in DD6 Single-Crystal Superalloy
XIE Hongji, LI Jiarong, LUO Yushi, ZHENG Sujie, LUO Kailun
图6 不同凝固条件下铸态DD6合金主元素的偏析比
Fig.6 Element segregation ratios of as-cast DD6 alloy under different solidification conditions
(a) Re, Co, and W (b) Al, Cr, Ta, Nb, and Ni