凝固条件对DD6单晶高温合金组织演化的影响 |
| 谢洪吉, 李嘉荣, 骆宇时, 郑素杰, 骆凯伦 |
|
Effect of Solidification Conditions on Microstructure Evolution in DD6 Single-Crystal Superalloy |
| XIE Hongji, LI Jiarong, LUO Yushi, ZHENG Sujie, LUO Kailun |
| 图2 不同凝固条件下铸态DD6合金显微组织的OM像 |
| Fig.2 OM images of the as-cast DD6 alloy under HRS process with pouring temperatures of 1500 oC (a, b), 1560 oC (c, d), and 1590 oC (e, f), and LMC process of 1590 oC (g, h) (a, c, e, g) transverse sections (b, d, f, h) longitudinal sections |
|