聚片孪生功能基元序构的高性能TiAl合金 |
| 陈光, 陈奉锐, 朱德民, 李贵忠, 李罗, 宋伟东, 王子特, 相恒高, 陈旸, 祁志祥 |
|
Polysynthetic Twinned High-Performance TiAl Alloy with Ordered Structures of Functional Units |
| CHEN Guang, CHEN Fengrui, ZHU Demin, LI Guizhong, LI Luo, SONG Weidong, WANG Zite, XIANG Henggao, CHEN Yang, QI Zhixiang |
| 图2 聚片孪生功能基元序构TiAl合金界面类型[ |