晶界沟槽形成过程的相场模拟
申文龙, 廖宇轩, 吴学志, 姜彦博, 柳文波

Phase-Field Simulation of Grain Boundary Groove Formation
SHEN Wenlong, LIAO Yuxuan, WU Xuezhi, JIANG Yanbo, LIU Wenbo
图4 相场模拟中不同时刻的沟槽轮廓与Mullins理论预测[7]的对比
Fig.4 Comparison of the normalized groove profile and Mullins' theory[7]