GH4169高温合金环轧过程组织模型适配性研究及应用 |
| 魏振, 李昕, 江河, 王川, 董建新 |
|
Microstructure Models Adaptability and Its Application in Ring Rolling Process of GH4169 Superalloy |
| WEI Zhen, LI Xin, JIANG He, WANG Chuan, DONG Jianxin |
| 图9 环轧后环锻件典型区域的局部取向差(KAM)分布图及等效塑性应变分布图 |
| Fig.9 Kernel average misorientation (KAM) distribution maps of typical locations 1 (a), 5 (b), and 8 (c) and effective plastic strain distribution map (d) of ring forging |
|