预先Mn配分对中锰钢中温连续冷却过程中贝氏体相变的影响
郑沁园, 刘朋, 路轶, 朱海龙, 郑成武, 栾义坤, 李殿中

Effect of Mn Pre-Partitioning on Bainite Transformation During Medium-Temperature Continuous Cooling of Medium Mn Steel
ZHENG Qinyuan, LIU Peng, LU Yi, ZHU Hailong, ZHENG Chengwu, LUAN Yikun, LI Dianzhong
图8 以不同起始冷却温度连续冷却0.2C-3Mn-1.5Si中锰钢的工程应力-应变曲线和力学性能
Fig.8 Engineering stress-strain curves (a) and mechanical properties (b) of the intercritically pre-annealed 0.2C-3Mn-1.5Si MMnS continu-ously cooled from different Ts at a cooling rate of 0.05 oC/s (YS—yield strength, UTS—ultimate tensile strength, TE—total elongation)