预先Mn配分对中锰钢中温连续冷却过程中贝氏体相变的影响 |
| 郑沁园, 刘朋, 路轶, 朱海龙, 郑成武, 栾义坤, 李殿中 |
|
Effect of Mn Pre-Partitioning on Bainite Transformation During Medium-Temperature Continuous Cooling of Medium Mn Steel |
| ZHENG Qinyuan, LIU Peng, LU Yi, ZHU Hailong, ZHENG Chengwu, LUAN Yikun, LI Dianzhong |
| 图5 临界区预退火0.2C-3Mn-1.5Si中锰钢在中温连续冷却过程中冷却至395、390和370 ℃时微观组织的SEM像和EBSD像 |