Cr对FeWB块体金属玻璃热稳定性和耐腐蚀性能的影响 |
| 肖思明, 刘天豪, 苏辰, 郭胜锋 |
|
Effect of Chromium on Thermal Stability and Corrosion Resistance in FeWB Bulk Metallic Glasses |
| XIAO Siming, LIU Tianhao, SU Chen, GUO Shengfeng |
| 图5 不同Cr含量FeCrWB合金在3.5%NaCl溶液中的电化学阻抗谱(EIS)以及等效电路图 |
| Fig.5 Nyquist plots (Inset is a locally enlarged riew) (a), Bode phase plots (b), Bode plots (c), and equivalent circuit diagram (d) of FeCrWB alloys in 3.5%NaCl solution (Z'—real part of impedance; Z"—imaginary part of impedance; |Z|—modulus of impedance; R1—solution resistance; R2—charge transfer resistance; R3—passive film resistance; Ws—Weber resistance; CPE, CPE1, and CPE2—constant phase elements) |
|