GH4151难变形高温合金的拉伸行为及其断裂失效机制 |
| 崔天亮, 谢兴飞, 温晓灿, 吕少敏, 曲敬龙, 杜金辉 |
|
Tensile Behavior and Fracture Mechanism of Hard-to-Deform GH4151 Superalloy |
| CUI Tianliang, XIE Xingfei, WEN Xiaocan, LYU Shaomin, QU Jinglong, DU Jinhui |
| 图10 550 ℃拉伸后GH4151合金断口纵截面的SEM像、EDS面分布图和TEM像 (b) BF image (c) DF image |
| Fig.10 Longitudinal SEM image and EDS elemental mappings (a) and TEM images (b, c) of the fracture morphology of GH4151 alloy after tensile testing at 550 oC |
|