GH4151难变形高温合金的拉伸行为及其断裂失效机制 |
| 崔天亮, 谢兴飞, 温晓灿, 吕少敏, 曲敬龙, 杜金辉 |
|
Tensile Behavior and Fracture Mechanism of Hard-to-Deform GH4151 Superalloy |
| CUI Tianliang, XIE Xingfei, WEN Xiaocan, LYU Shaomin, QU Jinglong, DU Jinhui |
| 图9 23~550 ℃拉伸过程中GH4151合金断裂过程示意图 |
| Fig.9 Schematics of fracture processes of GH4151 alloys during tensile testing at 23-550 oC (σ—tensile stress) |
|