高温无氧轧制Cu/1060Al/Cu三层复合材料的力学和导电性能 |
| 蒋志达, 胥杨洋, 于佳新, 刘文才, 朱浩文, 吴国华, 尚郑平 |
|
Mechanical and Conductive Properties of Cu/1060Al/Cu Three-Layer Composite Prepared by High-Temperature Oxygen-Free Rolling |
| JIANG Zhida, XU Yangyang, YU Jiaxin, LIU Wencai, ZHU Haowen, WU Guohua, SHANG Zhengping |
| 图9 退火态Cu/1060Al/Cu三层复合材料拉伸断裂机理示意图 |
| Fig.9 Schematics of tensile fracture mechanism of annealed Cu/1060Al/Cu three-layer composite (a) initial state (b) dislocation plugging (c) cracks initiation in IMCs (d) crack propagation and fracture |
|