Zr含量对Al-Mg-Si铸轧薄板再结晶行为和力学性能的影响
孙玉崇, 刘志敏, 徐振, 田双永, 田爽

Effect of Zr Content on Recrystallization Behavior and Mechanical Properties of Al-Mg-Si Cast-Rolled Sheet
SUN Yuchong, LIU Zhimin, XU Zhen, TIAN Shuangyong, TIAN Shuang
图3 不同Zr含量Al-Mg-Si铸轧板显微组织的SEM像
Fig.3 SEM images of Al-Mg-Si cast-rolled sheets with different Zr contents (Black arrows represent Al0.3Fe3Si0.7 phases, white arrows represent Mg2Si phases, red arrows represent Al17Fe3.2Mn0.8Si2 phases. Insets in Figs.3a, c, and e represent EDS results of the areas marked by the white rectangles, inset in Fig.3d is the corresponding enlarged view)