自然时效对新型Al-Zn-Mg-Cu合金人工时效行为的影响 |
| 姜磊, 周泰文韬, 张鑫彪, 肖星宇, 张志豪, 谢建新 |
|
Effect of Natural Aging on the Artificial Aging Behavior of a New Al-Zn-Mg-Cu Alloy |
| JIANG Lei, ZHOU Taiwentao, ZHANG Xinbiao, XIAO Xingyu, ZHANG Zhihao, XIE Jianxin |
| 图3 经不同时间自然时效及120 ℃人工时效不同时间后新型铝合金的硬度和人工峰值时效试样的工程应力-应变曲线 |
| Fig.3 Hardnesses of the new aluminum alloy after different natural aging time followed by artificial aging at 120 oC for different time (a) and engineering stress-strain curves under artificial peak aging (b) (The samples with natural aging of 0, 1, 7, and 30 d following with artificial aging are named NA0, NA1, NA7, and NA30, respectively) |
|