超声辅助下Mg/Mg-Zn-Al钎焊界面行为的分子动力学模拟 |
| 江国龙, 周霞 |
|
Molecular Dynamics Simulation on the Interfacial Behavior of Mg/Mg-Zn-Al Brazing with Ultrasonic Assistance |
| JIANG Guolong, ZHOU Xia |
| 图12 不同超声频率下母材和钎料的扩散系数及Mg/Mg-Zn-Al界面厚度 |
| Fig.12 Diffusion coefficients of solder (a) and BM (b) and thickness of Mg/Mg-Zn-Al interface (c) under different ultrasonic frequencies |
|