Sc在镍基变形高温合金BYG36真空感应熔炼中的烧损机制 |
| 闫静, 张佳丽, 邓睿, 何洋, 文新理, 章清泉, 乔利杰 |
|
Burning Loss Mechanism of Sc During Vacuum Induction Melting of Nickel-Based Superalloys |
| YAN Jing, ZHANG Jiali, DENG Rui, HE Yang, WEN Xinli, ZHANG Qingquan, QIAO Lijie |
| 图1 真空感应熔炼系统示意图和样品实物照片 |
| Fig.1 Schematic of the vacuum induction melting system (1—furnace cover, 2—crucible, 3—heater, 4—rotator, 5—liquid metal, 6—thermocouple, 7—observation window, 8—sprue, 9—entry nozzle, 10—mold) (a) and photos of samples taken from residue on the inner side surface of the crucible (b), residue on the crucible rim (c), residue on the inner side surface of the sprue (d), and residue on the inner surface of the entry nozzle (e) |
|