一种含稀土新型第四代镍基单晶高温合金的高温氧化行为和 γ' 相稳定性
郭世佳, 李健乐, 袁圣云, 李志刚, 于连旭, 张勇

High-Temperature Oxidation Behaviors and γ' Phase Stability of a New Fourth-Generation Single Crystal Superalloy with Rare Earth
GUO Shijia, LI Jianyue, YUAN Shengyun, LI Zhigang, YU Lianxu, ZHANG Yong
表1 图4中点1~6的EDS成分分析结果 (atomic fraction / %)
Table 1 EDS compositional analysis results of the points 1-6 in Fig.4
PointONiAlWTaYCeLaNdRuOxide
148.331.316.5-0.150.12---0.10Spinel
269.38.67.70.88.400.60---0.08TaO2
360.413.37.67.33.20-0.06--0.09NiWO4
474.67.310.40.40.070.08---8.80RuO2
556.512.520.91.21.500.20---0.06NiAl2O4
653.615.92.52.618.500.400.090.10.05-Spinel