晶界碳化物和动态再结晶对690合金柱状晶凝固组织高温塑性的影响
赵霞, 王旻, 郝宪朝, 张龙, 高明, 马颖澈, 刘奎

Effect of Grain Boundary Carbide and Dynamic Recrystalli-zation on the High-Temperature Plasticity of Columnar-Grain Solidified Microstructure in 690 Alloy
ZHAO Xia, WANG Min, HAO Xianchao, ZHANG Long, GAO Ming, MA Yingche, LIU Kui
图13 高温拉伸过程中690合金柱状晶试样晶界碳化物和再结晶对裂纹扩展行为影响示意图
Fig.13 Schematics of the influence of grain boundary carbides and recrystallization on crack propagation behavior of 690 alloy columnar-grain samples after tensile test at 900-1050 oC (a), 1100 oC (b), 1150-1200 oC (c), and 1250 oC (d)