晶界碳化物和动态再结晶对690合金柱状晶凝固组织高温塑性的影响
赵霞, 王旻, 郝宪朝, 张龙, 高明, 马颖澈, 刘奎

Effect of Grain Boundary Carbide and Dynamic Recrystalli-zation on the High-Temperature Plasticity of Columnar-Grain Solidified Microstructure in 690 Alloy
ZHAO Xia, WANG Min, HAO Xianchao, ZHANG Long, GAO Ming, MA Yingche, LIU Kui
图11 铸态和固溶态690合金柱状晶试样中晶界碳化物的SEM像
Fig.11 SEM images of grain boundary carbides in the 690 alloy columnar-grain samples under as-cast state (a) and annealed at 1000 oC (b), 1050 oC (c), 1100 oC (d), and 1150 oC (e) for 10 min