晶界碳化物和动态再结晶对690合金柱状晶凝固组织高温塑性的影响 |
| 赵霞, 王旻, 郝宪朝, 张龙, 高明, 马颖澈, 刘奎 |
|
Effect of Grain Boundary Carbide and Dynamic Recrystalli-zation on the High-Temperature Plasticity of Columnar-Grain Solidified Microstructure in 690 Alloy |
| ZHAO Xia, WANG Min, HAO Xianchao, ZHANG Long, GAO Ming, MA Yingche, LIU Kui |
| 图9 690合金柱状晶试样高温拉伸口附近区域(距断口约7 mm处)的TEM像和SAED花样 |
| Fig.9 TEM images of dislocation morphologies on the region near the fracture surface (≈ 7 mm) of 690 alloy columnar-grain samples after tensile testing at 1000 oC (a), 1100 oC (b), and 1200 oC (c) (Insets in Figs.9a-c are selected area electron diffraction (SAED) patterns) |
|