GH4738镍基高温合金O累积程度对疲劳性能与晶界损伤的影响及表征
赵晓, 徐超, 江河, 姚志浩, 董建新

Effect and Characterization of O Accumulation Degree on Fatigue Properties and Grain Boundary Damage in GH4738 Ni-Based Superalloy
ZHAO Xiao, XU Chao, JIANG He, YAO Zhihao, DONG Jianxin
图5 700 ℃时效前后GH4738合金中γ'相形貌的SEM像
Fig.5 SEM images of γ' phase morphologies in GH4738 alloy
(a) non-aging
(b) aged at 700 oC for 1000 h