GH4738镍基高温合金O累积程度对疲劳性能与晶界损伤的影响及表征 |
| 赵晓, 徐超, 江河, 姚志浩, 董建新 |
|
Effect and Characterization of O Accumulation Degree on Fatigue Properties and Grain Boundary Damage in GH4738 Ni-Based Superalloy |
| ZHAO Xiao, XU Chao, JIANG He, YAO Zhihao, DONG Jianxin |
| 图3 700 ℃时效不同时间后GH4738合金的室温疲劳裂纹扩展曲线 |
| Fig.3 Room temperature FCG curves of GH4738 alloy aged at 700 oC for different time (a) FCG cycle curves (b) FCG rate curves |
|