高温合金定向凝固雀斑形成机理及控制技术研究进展
|
|
贾玉亮, 张勇佳, 史泽楷, 沈旭, 殷亚军, 施长坤, 周建新, 吕志刚
|
Review of the Formation Mechanism and Control Technology for Freckle Defects in Directionally Solidified Superalloys
|
|
JIA Yuliang, ZHANG Yongjia, SHI Zekai, SHEN Xu, YIN Yajun, SHI Changkun, ZHOU Jianxin, LYU Zhigang
|
|
表2 已报道部分雀斑试样的尺寸、抽拉速率及合金成分特征[9,30,58~60,72,73]
|
Table 2 Sample size, withdrawal rate, and alloy composition of sample with freckles in the literatures [9,30,58-60,72,73]
|
|
| Content of W, Re, and Al in nickel-based alloys* | Dimension | Withdrawal rate | Ref. |
|---|
Mar-M200: 13.2W-4.9Al... Udimet700: 4.19Al... | ϕ101.6 mm | - | [9] | | CMSX-4: 6W-3Re-5.6Al... | Thickness: 10 mm | 1, 6 mm·min-1 (Intense freckle occurs at a rate of 1 mm·min-1) | [72] | | DD33: 6W-4Re-6Al... | Thickness: 0.6-10 mm (Freckles tendency inward) | 1, 3, 6 mm·min-1 (Intense freckle occurs at a rate of 1 mm·min-1) | [59] | | CMSX-4: 6W-3Re-5.6Al... | 20 mm × 40 mm × 50 mm | 1.2, 4.2 mm·min-1 (Intense freckle occurs at a rate of 1.2 mm·min-1) | [73] | | CMSX-4: 6W-3Re-5.6Al... | Nearly ϕ20 mm (Freckles tendency inward) | 1 mm·min-1 | [58] | | PW1483: 1.81W-3.63Al... | Nearly ϕ15 mm (Freckles tendency inward) | 1 mm·min-1 | [60] | | 6.52W-4.89Re-5.69Al... | 60 mm × 25 mm × 150 mm (Freckles tendency inward) | 1.5 mm·min-1 | [30] |
|
|
|