高温合金定向凝固雀斑形成机理及控制技术研究进展
贾玉亮, 张勇佳, 史泽楷, 沈旭, 殷亚军, 施长坤, 周建新, 吕志刚

Review of the Formation Mechanism and Control Technology for Freckle Defects in Directionally Solidified Superalloys
JIA Yuliang, ZHANG Yongjia, SHI Zekai, SHEN Xu, YIN Yajun, SHI Changkun, ZHOU Jianxin, LYU Zhigang
图3 不同合金叶片上的雀斑分布[18]
Fig.3 Distributions of freckle chains on blades with different alloy compositions[18]
(a) UCSX6 (b) UCSX7 (On the basis of UCSX6, add 1.5%Cr and 3.0%Mo, mass fraction)
(c) UCSX8 (On the basis of UCSX7, add 2% Ta, and reduce 2%W and 0.8%Re, mass fraction)