先进导电铜基复合材料设计与制备研究进展
姜伊辉, 张兴德, 石浩, 曹飞, 马文君, 王艳芳, 梁淑华

Research Progress in the Design and Preparation of Advanced Conductive Copper Matrix Composites
JIANG Yihui, ZHANG Xingde, SHI Hao, CAO Fei, MA Wenjun, WANG Yanfang, LIANG Shuhua
图3 铜基复合材料的增材制造技术[28,33]
Fig.3 Additive manufacturing technologies of copper matrix composites (a, b) repeated hot and cold cycles during printing (a) and compression-tension simulation generated by the printing process (b)[28] (σXX, σYY, and σZZ are stress components) (c-g) microstructures (c), mechanical (d) and conductivity (e) properties, heat transfer during printing (f), and products (g) of Cu-Cr-Nb alloy formed by additive manufacturing[33] (LPBF—laser powder-bed-fusion)