先进导电铜基复合材料设计与制备研究进展
姜伊辉, 张兴德, 石浩, 曹飞, 马文君, 王艳芳, 梁淑华

Research Progress in the Design and Preparation of Advanced Conductive Copper Matrix Composites
JIANG Yihui, ZHANG Xingde, SHI Hao, CAO Fei, MA Wenjun, WANG Yanfang, LIANG Shuhua
图2 铜基复合材料的喷射沉积技术 [21,22]
Fig.2 Schematics and microstructures of liquid-solid[21] (a) and liquid-liquid[22] (b) reactive spray deposition technologies of copper matrix composites