赵子博, 谭海兵, 张博华, 刘玉敬, 刘建荣, 郭会明, 曾卫东, 田伟, 王清江

Review: Microtextures in Near α and α + β Dual-Phase Titanium Alloys
ZHAO Zibo, TAN Haibing, ZHANG Bohua, LIU Yujing, LIU Jianrong, GUO Huiming, ZENG Weidong, TIAN Wei, WANG Qingjiang
图9 Ti60合金在热处理过程中的αp/β相界演化及其对组织的影响[26,69]
Fig.9 Evolutions of the αp/β phase boundary and its effects on microstructure during heat treatment of Ti60 alloy[26,69] (a1, a2) Burgers orientation relationship (BOR) deviation angle (θ) distributions between αp grains and the neighboring β grains at 1030 oC (a1) and 1040 oC (a2) (fθ ≤ 10° denotes the number fraction of θ ≤ 10°)(b) band contrast (BC) map of αp grains with some special phase boundaries (GB—grain boundary)(c) schematic of β grain boundary (between grains A and B) pinning by an αp particle (particle C), showing the relevent interfacial energies (γAB, γAC, and γBC denote the interfacial energies of grains A and B, grain A and particle C, and grain B and particle C, respectively)