燃料电池金属双极板的研究进展与展望
罗海文, 林雄, 刘高阳, 胡斌

Progress and Perspectives on Metallic Bipolar Plates in Fuel Cells
LUO Haiwen, LIN Xiong, LIU Gaoyang, HU Bin
表7 铁素体不锈钢的化学成分[58~62] (mass fraction / %)
Table 7 Chemical compositions of ferritic stainless steels[58-62]
GradeCrNiMnSiMoOthersFe
SS43016-180.751.001.00-C < 0.12Bal.
SS43417.946-0.2890.2850.938C < 0.12Bal.
SS43618.101-0.5050.3701.037Nb = 0.3, Ti = 0.2Bal.
SS44118.230-0.5190.5060.033Nb = 0.69, Ti = 0.27Bal.
SS44418.485-0.1860.3821.763Ti + Nb ≤ 0.80Bal
SS44628.3672.9580.4340.4243.502Ti + Nb ≤ 0.75Bal.
SS446M26.630.183< 1.50< 1.002.04Ti < 0.06, Cu < 0.50, C < 0.004, P < 0.005, S < 0.005Bal.
Fe20Cr4V20.29-0.080.06-C < 0.05, S < 0.001, V = 3.91Bal.
POS470FC25-320.50.20.4-C < 0.02, P < 0.04, S < 0.03, Cu = 2.0Bal.