金属材料强度-塑性及强度-电导率定量关系 |
| 张哲峰, 侯嘉鹏, 刘睿, 李孝滔, 张振军, 张鹏 |
|
Quantitative Relationships Between the Strength-Plasticity and Strength-Electrical Conductivity of Metallic Materials |
| ZHANG Zhefeng, HOU Jiapeng, LIU Rui, LI Xiaotao, ZHANG Zhenjun, ZHANG Peng |
| 图4 高强-高导金属导线微观组织设计三原则示意图,以及细长晶粒特征参数[ |
| Fig.4 Schematics of three principles including fine-long grains, hard texture (L—length of elongated grain, t—width of grain) (a) and nano-scale precipitates (b) for designing metallic conductors with high strength and high electrical conductivity; and quantitative models for strength and electrical conductivity (EC) relating to elongated grain parameters[ |
|