表3 相关参数计算结果
Table 3 Calculation results of parameters
SteelVm / (m3⋅mol-1)ΔGv / (J⋅m-3)r* / mΔG* / JQC / J
0Cr7.2958 × 10-6-5.0906 × 1071.9644 × 10-88.0821 × 10-162.4410 × 10-19
1Cr7.2963 × 10-6-4.5379 × 1072.2037 × 10-810.1707 × 10-162.4842 × 10-19