Cr对低碳含Ti微合金钢奥氏体等温分解行为的影响
熊杰, 蓝慧芳, 李林鲜, 唐帅, 刘振宇, 王国栋

Effect of Cr on the Isothermal Decomposition Behavior of Austenite in Low-Carbon Ti-Bearing Microalloyed Steel
XIONG Jie, LAN Huifang, LI Linxian, TANG Shuai, LIU Zhenyu, WANG Guodong
表1 实验用钢的化学成分及奥氏体转变结束温度(Ae1)和开始温度(Ae3)
Table 1 Chemical compositions of the experimental steels and finish temperature (Ae1) and start temperature (Ae3) of austenite transformation
SteelMass fraction / %

Ae1

oC

Ae3

oC

CMnSiTiCrNOFe
0Cr0.0931.710.1070.072–0.00460.0013Bal.668822
1Cr0.1121.750.0850.0710.980.00380.0012Bal.684805