Cr对低碳含Ti微合金钢奥氏体等温分解行为的影响
熊杰, 蓝慧芳, 李林鲜, 唐帅, 刘振宇, 王国栋

Effect of Cr on the Isothermal Decomposition Behavior of Austenite in Low-Carbon Ti-Bearing Microalloyed Steel
XIONG Jie, LAN Huifang, LI Linxian, TANG Shuai, LIU Zhenyu, WANG Guodong
图8 铁素体生长过程中γ/α界面移动距离和移动速率的DICTRA模拟结果
Fig.8 DICTRA simulation results of the migration distance (a) and migration rate (b) of the γ/α interface during the growth process of ferrite (Inset in Fig.8b is the corresponding enlarged view)