Cr对低碳含Ti微合金钢奥氏体等温分解行为的影响 |
| 熊杰, 蓝慧芳, 李林鲜, 唐帅, 刘振宇, 王国栋 |
|
Effect of Cr on the Isothermal Decomposition Behavior of Austenite in Low-Carbon Ti-Bearing Microalloyed Steel |
| XIONG Jie, LAN Huifang, LI Linxian, TANG Shuai, LIU Zhenyu, WANG Guodong |
| 图5 不同温度和Cr含量下实验用钢的Gibbs自由能(G)和两相Gibbs自由能差(ΔGγ→α) |
| Fig.5 Gibbs free energy (G) (a) and Gibbs free energy difference (ΔG) of γ→α transformation (ΔGγ→α ) (b) of experimental steel under different temperatures, partially enlarged view of Fig.5b (c), and ΔG (d) of experimental steel under different Cr contents (ΔGγ→α = Gα - Gγ, Gα, Gγ —G of α and γ phase, respectively; Δ—difference in ΔG between 0Cr and 1Cr steels at 650 oC) |
|