高温钛合金中合金原子在 α2 相中占位选择的第一性原理研究 |
|||||||||
| 梁弼宁, 曹烁, 王慈, 刘建荣, 杨锐, 胡青苗 | |||||||||
|
Site Occupation of Alloying Elements in α2 Phase in High-Temperature Titanium Alloys: A First-Principles Study |
|||||||||
| LIANG Bining, CAO Shuo, WANG Ci, LIU Jianrong, YANG Rui, HU Qingmiao | |||||||||
| 表1 高温钛合金中α与α2相平衡时Ti和Al的化学势与二者单质状态的化学势(μTi和μAl) (eV) |
|||||||||
| Table 1 Chemical potentials of Ti and Al (μTi and μAl) calculated considering the phase equilibrium between the α and α2 phases in high-temperature titanium alloy, in comparison with those taken as the energies of Ti and Al in their elemental states |
|||||||||
|
|||||||||