高温钛合金中合金原子在 α2 相中占位选择的第一性原理研究
梁弼宁, 曹烁, 王慈, 刘建荣, 杨锐, 胡青苗

Site Occupation of Alloying Elements in α2 Phase in High-Temperature Titanium Alloys: A First-Principles Study
LIANG Bining, CAO Shuo, WANG Ci, LIU Jianrong, YANG Rui, HU Qingmiao
图2 高温钛合金中α-Ti与α2两相平衡时第三~第六周期合金元素在α2相中Ti及Al亚点阵上的分配系数(k)随温度的变化
Fig.2 Partition coefficients (k) of alloying elements on the Ti and Al sublattices of α2 equilibrium with α-Ti in high-temperature titanium alloy, as func-tions of temperature
(a) third and fourth period elements
(b) fifth period elements
(c) sixth period elements