预时效对Al-Zn-Mg-Cu合金热变形行为与微观组织演变规律的影响
王振瑜, 石全强, 范然, 崔丽, 王威

Effects of Preaging Treatment on the Hot Deformation Behavior and Microstructural Evolution of Al-Zn-Mg-Cu Alloys
WANG Zhenyu, SHI Quanqiang, FAN Ran, CUI Li, WANG Wei
表1 固溶态和时效态Al-Zn-Mg-Cu合金在0.01 s-1应变速率下573和673 K时变形晶粒、亚结构和再结晶晶粒占比统计
Table 1 Statistics on the proportion of deformed grains, substructures, and recrystallized grains in solid-solution and aging state Al-Zn-Mg-Cu alloys at strain rate of 0.01 s-1 and temperatures of 573 and 673 K
Temperature / KState

Volume fraction of

deformed grains / %

Volume fraction of

substructures / %

Volume fraction of

recrystallized grains / %

573Solid-solution75.721.23.1
Aging98.00.91.1
673Solid-solution52.323.624.1
Aging62.025.812.2