预时效对Al-Zn-Mg-Cu合金热变形行为与微观组织演变规律的影响
王振瑜, 石全强, 范然, 崔丽, 王威

Effects of Preaging Treatment on the Hot Deformation Behavior and Microstructural Evolution of Al-Zn-Mg-Cu Alloys
WANG Zhenyu, SHI Quanqiang, FAN Ran, CUI Li, WANG Wei
图9 743 K、不同应变速率下,固溶态和时效态Al-Zn-Mg-Cu合金的微观组织EBSD分析
Fig.9 EBSD analyses of solid-solution state (a1-a4, b1-b4) and aging state (c1-c4, d1-d4) Al-Zn-Mg-Cu alloys at 743 K with strain rates of 0.01 s-1 (a1-a4, c1-c4) and 0.50 s-1 (b1-b4, d1-d4) (GDRX—geometric dynamic recrystallization)
(a1-d1) IPF maps (DRX grains are shown in the boxes) (a2-d2) grain boundary maps (a3-d3) KAM maps (a4-d4) recrystallization maps (Blue for recrystallized grains, yellow for substructures, and red for deformed grains)