预时效对Al-Zn-Mg-Cu合金热变形行为与微观组织演变规律的影响 |
| 王振瑜, 石全强, 范然, 崔丽, 王威 |
|
Effects of Preaging Treatment on the Hot Deformation Behavior and Microstructural Evolution of Al-Zn-Mg-Cu Alloys |
| WANG Zhenyu, SHI Quanqiang, FAN Ran, CUI Li, WANG Wei |
| 图8 673 K、0.01 s-1应变速率下,固溶态和时效态Al-Zn-Mg-Cu合金微观组织的TEM像 |
| Fig.8 TEM images of solid-solution state (a-c) and aging state (d-f) Al-Zn-Mg-Cu alloys at 673 K and (a, d) morphologies of DRX grains (b, c) morphologies between precipitates (b) and double-wall microbands (c) (e) interaction between fine precipitates and dislocations (f) discontinuous coarsening of precipitates |
|