预时效对Al-Zn-Mg-Cu合金热变形行为与微观组织演变规律的影响
王振瑜, 石全强, 范然, 崔丽, 王威

Effects of Preaging Treatment on the Hot Deformation Behavior and Microstructural Evolution of Al-Zn-Mg-Cu Alloys
WANG Zhenyu, SHI Quanqiang, FAN Ran, CUI Li, WANG Wei
图7 673 K、0.01 s-1应变速率下,固溶态和时效态Al-Zn-Mg-Cu合金微观组织EBSD分析
Fig.7 EBSD analyses of solid-solution state (a1-a4) and aging state (b1-b4) Al-Zn-Mg-Cu alloys at 673 K and ε˙ = 0.01 s-1
(a1, b1) IPF maps (DRX grains are shown in the boxes) (a2, b2) grain boundary maps (a3, b3) KAM maps (a4, b4) recrystallization maps (Blue for recrystallized grains, yellow for substructures, and red for deformed grains)