预时效对Al-Zn-Mg-Cu合金热变形行为与微观组织演变规律的影响
王振瑜, 石全强, 范然, 崔丽, 王威

Effects of Preaging Treatment on the Hot Deformation Behavior and Microstructural Evolution of Al-Zn-Mg-Cu Alloys
WANG Zhenyu, SHI Quanqiang, FAN Ran, CUI Li, WANG Wei
图4 473 K、0.01 s-1应变速率下,固溶态和时效态Al-Zn-Mg-Cu合金微观组织的TEM像
Fig.4 TEM images of solid-solution state (a, b) and aging state (c, d) Al-Zn-Mg-Cu alloys at 473 K and ε˙ = 0.01 s-1
(a, c) morphologies of precipitates and dislocation entanglement (GP—Guinier-Preston) (b, d) morphologies of precipitation free zone