预时效对Al-Zn-Mg-Cu合金热变形行为与微观组织演变规律的影响
王振瑜, 石全强, 范然, 崔丽, 王威

Effects of Preaging Treatment on the Hot Deformation Behavior and Microstructural Evolution of Al-Zn-Mg-Cu Alloys
WANG Zhenyu, SHI Quanqiang, FAN Ran, CUI Li, WANG Wei
图3 固溶态和时效态Al-Zn-Mg-Cu合金的应力-应变曲线及固溶态与时效态合金的流变应力差曲线
Fig.3 Stress-strain curves of Al-Zn-Mg-Cu alloys under solid-solution and aging states (a-c) and differences in rheological stress of alloys between solid-solution state and aging state (d)
(a) ε˙ = 0.01 s-1, room temperature compression
(b) ε˙ = 0.01 s-1, 473-743 K compression
(c) ε˙ = 0.50 s-1, 473-743 K compression (Inset shows the enlargement of the dotted box)