预时效对Al-Zn-Mg-Cu合金热变形行为与微观组织演变规律的影响 |
| 王振瑜, 石全强, 范然, 崔丽, 王威 |
|
Effects of Preaging Treatment on the Hot Deformation Behavior and Microstructural Evolution of Al-Zn-Mg-Cu Alloys |
| WANG Zhenyu, SHI Quanqiang, FAN Ran, CUI Li, WANG Wei |
| 图2 固溶态和时效态Al-Zn-Mg-Cu合金的初始微观组织表征 |
| Fig.2 Original microstructure characterizations of solid-solution state (a1-a3, c1-c3) and aging state (b1-b3, d1-d3) Al-Zn-Mg-Cu alloys (HAGB—high-angle grain boundary, > 15o; LAGB—low-angle grain boundary, 2o-10o; MAGB—medium-angle grain boundary, 10o-15o. The significance of the color representation of inverse pole figure (IPF) and kernel average misorientation (KAM) plots in this paper is consistent with Figs.2a1 and a3, respectively) (a1, b1) IPF maps (a2, b2) grain boundary orientation difference maps (a3, b3) KAM maps (The average KAM values are provided in the upper-right corner) (c1, d1) TEM images (c2, d2) EDS mappings (c3, d3) HRTEM images and corresponding fast Fourier transform (FFT) images of the box areas |
|