镁离子电池用Mg-0.1Sn负极材料的组织特征和电化学行为 |
| 李瑜, 程伟丽, 穆映洲, 王利飞, 王红霞, 崔泽琴, 张全福, 宋蕾, 余晖 |
|
Microstructural Characteristics and Electrochemical Behavior of a Mg-0.1Sn Anode for Magnesium-Ion Batteries |
| LI Yu, CHENG Weili, MU Yingzhou, WANG Lifei, WANG Hongxia, CUI Zeqin, ZHANG Quanfu, SONG Lei, YU Hui |
| 图3 不同电流密度和沉积容量下P-Mg//P-Mg和T0//T0对称电池的沉积-溶解曲线和沉积容量为1.0 mA⋅h/cm2时不同电流密度下的倍率性能 |
| Fig.3 Deposition-dissolution curves of P-Mg//P-Mg and T0//T0 symmetric cells under different current densities and deposition capacities of 1.0 mA/cm2, 0.5 mA⋅h/cm2 (a), 1.0 mA/cm2, 1.0 mA⋅h/cm2 (b), 4.0 mA/cm2, 1.0 mA⋅h/cm2 (c), and 5.0 mA/cm2, 1.25 mA⋅h/cm2 (d); rate performances under different current densities with deposition capacity of 1.0 mA⋅h/cm2 (e) |
|