Ti掺杂的SmFe12 基纳米晶永磁合金物相组成和组织性能 |
| 程锋, 吕皓, 刘雪梅, 宋晓艳 |
|
Phase Constitution, Microstructure, and Properties of Ti-Doped SmFe12-Based Nanocrystalline Permanent Magnetic Alloys |
| CHENG Feng, LU Hao, LIU Xuemei, SONG Xiaoyan |
| 图8 纳米晶SmFe11Ti1合金经不同淬火工艺后的物相组成和磁性能 |
| Fig.8 Phase constitution and magnetic properties of nanocrystalline SmFe11Ti1 alloy prepared by different quenching processes (a) XRD patterns of alloys after different quenching processes (b) effect of quenching process on the ratio of 1∶12 phase and α-Fe phase in the alloy (c) hysteresis loops of SmFe11Ti1 bulks obtained from different quenching processes (Inset is the local enlarged diagram) (d) magnetic property data read from the hysteresis loop in Fig.8c |
|