Ti掺杂的SmFe12 基纳米晶永磁合金物相组成和组织性能
程锋, 吕皓, 刘雪梅, 宋晓艳

Phase Constitution, Microstructure, and Properties of Ti-Doped SmFe12-Based Nanocrystalline Permanent Magnetic Alloys
CHENG Feng, LU Hao, LIU Xuemei, SONG Xiaoyan
图7 680 ℃烧结得到的SmFe11Ti1试样的微观组织结构分析
Fig.7 Microstructure analyses of the SmFe11Ti1 sample sintered samples at 680 oC
(a) bright field TEM image (Inset is the statistical result of grain size distribution)
(b) SAED pattern (Left image is the local bright field image)
(c) HRTEM image
(d) HRTEM image and FFT (inset) of the rectangle region in Fig.7c