Ti掺杂的SmFe12 基纳米晶永磁合金物相组成和组织性能 |
| 程锋, 吕皓, 刘雪梅, 宋晓艳 |
|
Phase Constitution, Microstructure, and Properties of Ti-Doped SmFe12-Based Nanocrystalline Permanent Magnetic Alloys |
| CHENG Feng, LU Hao, LIU Xuemei, SONG Xiaoyan |
| 图3 不同高能球磨时间下SmFe11Ti1粉末的XRD谱及球磨4 h后粉末的HRTEM像和SAED花样 |
| Fig.3 Effects of high-energy ball milling time on the phase constitution of SmFe11Ti1 powder (a) XRD patterns of the powder after different ball milling time(b) HRTEM image of the powder and SAED pattern (inset) after ball milling for 4 h (d—interplanar spacing) |
|