Ti掺杂的SmFe12 基纳米晶永磁合金物相组成和组织性能
程锋, 吕皓, 刘雪梅, 宋晓艳

Phase Constitution, Microstructure, and Properties of Ti-Doped SmFe12-Based Nanocrystalline Permanent Magnetic Alloys
CHENG Feng, LU Hao, LIU Xuemei, SONG Xiaoyan
图2 SmFe12 - x Ti x (x = 0、0.5、1、1.5和2)铸态合金第一象限和第二象限部分的磁滞回线
Fig.2 Hysteresis loops of the SmFe12 - x Ti x (x = 0, 0.5, 1, 1.5, 2) ingots in the first and second quadrants (J—magnetic polarization, H—magnetic field intensity)