冷喷涂及后续热-机械处理制备高强度高导电性Cu-10Fe原位复合材料
胡晓娜, 陈威, 邹晋, 胡强, 陆德平, 马力

High-Strength and High-Conductivity Cu-10Fe In Situ Composites Fabricated via Cold Spraying and Subsequent Thermo-Mechanical Treatment
HU Xiaona, CHEN Wei, ZOU Jin, HU Qiang, LU Deping, MA Li
图1 Cu粉和Fe粉微观形貌的SEM像和粒径分布
Fig.1 SEM images (a, c) and particle size distributions (b, d) of Cu powder (a, b) and Fe powder (c, d) (D10—volume 10th percentile diameter, D50—volume median diameter, D90—volume 90th percentile diameter)