粉末特征对激光粉末床熔融制备可降解Zn-Mn-Mg合金组织与力学性能的影响
黄成聪, 李亚庚, 王鲁宁

Effects of Powder Morphology on Microstructure Evolution and Mechanical Properties of Laser Powder Bed Fusion Degradable Zn-Mn-Mg Alloy
HUANG Chengcong, LI Yageng, WANG Luning
图8 EIGA和PREP方法制备的合金粉末经LPBF工艺(P = 50 W、 V = 600 mm/s)成形后块体试样拉伸断口的SEM像
Fig.8 Low (a, b) and high (c, d) magnified SEM images showing the tensile fracture surfaces of bulk samples prepared via EIGA + LPBF (a, c) and PREP + LPBF (b, d) at P = 50 W, V = 600 mm/s